AK01-07 · 6 MIN · M01 MATERIALS · LESSON 7 OF 7

The most common material mistakes

Clicking loads the video from YouTube (youtube-nocookie.com).

Chapters

In short

  1. 01The sink unit is made from moisture-resistant board, or at least its bottom is well closed and protected.
  2. 02Every cut-out in a worktop is sealed before the sink and the hob are fitted.
  3. 03The fronts for one project are ordered all at once, because a decor from another batch can have a different shade.
  4. 04The grain is checked in the cutting list before cutting, not after.
  5. 05A long shelf needs a thicker board or a support in the middle. A thin shelf sags under load over time.
  6. 06The protective film on gloss fronts stays on until fitting is finished.
Video transcriptthe narration as text

Six material mistakes that only show once the kitchen is finished, when fixing them is expensive. For each one you'll see why it happens, and how to avoid it at the design stage.

Standard particleboard under the sink

Mistake one: a sink unit made of standard particleboard, with open edges. Drop by drop, over months, water from the pipes and the siphon gets into the edges of the bottom and the sides. The board swells, and swollen particleboard never goes back to its original shape.

So make the sink unit from moisture-resistant board. If that's not possible, at least close up and protect its bottom well: put edge tape on all the edges and seal the joints. When the sink or the tap is changed later, check the pipe joints again.

Check this in your own kitchen too: look at the bottom edges under the sink.

An unsealed worktop cut-out

Mistake two: a cut-out for the sink or the hob with no sealant. Water creeps under the rim of the sink, finds the open core, and the board around the cut-out swells. The laminate then lifts, and the worktop usually has to be replaced.

Every cut-out in a worktop is sealed before the sink and the hob go in. It's a quick job, and it protects the worktop for years. Seal the cut-out for the hob as well: there's less water there, but there's still steam, and things get spilled.

Fronts from different batches

Mistake three: fronts in the same decor, ordered at two different times. Batches of the same decor can differ slightly in their shade. On a single front you won't see it, but on two fronts side by side it shows at once.

That's why the fronts for one project are ordered all at once. If you do need to buy more later, compare a sample of the new batch with the fronts you already have before you order.

Grain the wrong way

Mistake four: a part cut with the grain the wrong way. It's often a drawer front, because it's wider than it is high, so it's easy to turn it the wrong way round.

A part cut with the grain the wrong way can't be fixed; it has to be cut again. So check the grain in the cutting list, before cutting, not when the customer notices. Take the drawing of the kitchen, and for every single front, check whether it's the height or the width that runs along the grain.

A long shelf from thin board

Mistake five: a long shelf made from thin board. An eighteen millimetre particleboard shelf, in a cabinet about one metre wide, slowly sags over time under the weight of the books on it. The same thing happens to shelves that hold heavy plates and pans.

The sag grows quickly with the span. A shelf that's twice as long doesn't sag twice as much, it sags far more.

Two things help: a thicker board, or a support in the middle that shortens the span. The support can be a divider, or a metal bracket under the middle of the shelf.

Edge tape and decor have no effect on sag. Neither a different decor nor thinner edge tape will help a shelf.

High gloss without film during fitting

Mistake six: the protective film taken off gloss fronts before the fitting is finished. Fitting means tools, ladders, dust and lots of hands on everything, and a gloss surface remembers every single scratch.

The film on gloss fronts stays on until fitting is finished. It comes off last, when the fronts are adjusted, the handles are on, and there's no more work around them.

In short

In short. Make the sink unit from moisture-resistant board, or at least close up and protect its bottom well. Seal every worktop cut-out before the sink and the hob go in. Order the fronts for one project all at once, because another batch can have a different shade. Check the grain in the cutting list before cutting, not after. A long shelf needs a thicker board or a support in the middle. And the protective film on gloss fronts stays on until fitting is finished.

In Easy Form Studio, type the board type for the sink unit into the cabinet's Note, for example moisture-resistant particleboard. The note goes into every row of that cabinet in the cutting list.

Check the grain in the cutting list before you send it to the saw: the Length always runs along the grain. On the PDF board drawing, a grey double arrow shows the grain direction. For a single board, you also see it in the Grain field.

You change the shelf thickness in the EFS Cabinet tab, in the Shelves panel. You add a divider that shortens the span with Shift and V. EFS doesn't calculate shelf sag, so decide the thickness and the span yourself.

The supplier order adds up all the boards by decor, so you can order the fronts all at once, for the whole project. The tutorials Cutting list and cut size, How a cabinet is built, and The production package and the supplier order show you how.

A three-question quiz and the summary are on the academy page, the link is below the video. That completes the Materials module. The next module is hardware: hinges, runners, flaps, handles and legs, and how to read a manufacturer's catalogue.